Detalhes do produto:
|
| Tipo de ligação: | Silício Modificado | Porosidade aparente: | 6% |
|---|---|---|---|
| Conteúdo de MgO: | 77% | Densidade aparente: | 2,98g/cm3 |
| Força de esmagamento frio: | 44 MPa | Refraturaz sob carga: | 1680 C |
| Teor fixo de carbono: | 12% | ||
| Destacar: | C12 AOD Sidewall Brick,Slag Resistant Lining Block,Stainless Refining Refractory |
||
The C12 grade balances 12% fixed carbon against 77% MgO so the brick carries heat through AOD sidewall duty without losing the matrix that holds the AOD converter lining together. Thermal cycling is the main wear driver in stainless refining, so the graphite network is allowed to bridge the magnesia grains instead of sitting in isolated pockets. That structure delivers 28 cycles of thermal shock without through-cracks, at a bulk density of 2.98 g/cm3 and 6% apparent porosity.
Pessoa de Contato: Mr. Pika
Telefone: 86-13838387996
Fax: 86-0371-56010932